Aliaje fuzibile
Aliajele fuzibile sunt aliaje cu puncte de topire la temperaturi ambientale. Un exemlu ar fi cele bazate pe galiu.
Exemple
| Compoziție - procent masic | °C | eutectic? | Nume sau remarcă |
|---|---|---|---|
| Cs 73.71, K 22.14, Na 4.14[1] | −78.2 | da | |
| Hg 91.5, Tl 8.5 | −58 | yes | folosit in termometre de temperaturi joase |
| Hg 100 | −38.8 | (da) | |
| Cs 77.0, K 23.0 | −37.5 | ||
| K 76.7, Na 23.3 | −12.7 | da | |
| K 78.0, Na 22.0 | −11 | nu | NaK |
| Ga 61 , In 25, Sn 13, Zn 1 | 8.5 | da | |
| Ga 62.5, In 21.5, Sn 16.0 | 10.7 | da | |
| Ga 69.8, In 17.6, Sn 12.5 | 10.8 | nu | |
| Ga 68.5, In 21.5, Sn 10 | 11 | no | Galinstan |
| Ga 75.5, In 24.5 | 15.7 | da | |
| Cs 100 | 28.6 | da | |
| Ga 100 | 29.8 | da | |
| Bi 40.3, Pb 22.2, In 17.2, Sn 10.7, Cd 8.1, Tl 1.1 | 41.5 | da | |
| Bi 40.63, Pb 22.1, In 18.1, Sn 10.65, Cd 8.2 | 46.5 | ||
| Bi 32.5, In 51.0, Sn 16.5 | 60.5 | yes | metalul lui Field |
| Bi 49.5, Pb 27.3, Sn 13.1, Cd 10.1 | 70.9 | yes | aliaj Lipowitz |
| Bi 50.0, Pb 25.0, Sn 12.5, Cd 12.5 | 71 | no | metal Wood |
| In 66.3, Bi 33.7 | 72 | da | |
| Bi 52.5, Pb 32.0, Sn 15.5 | 95 | da | |
| Bi 50.0, Pb 31.2, Sn 18.8 | 97 | nu | metalul lui Newton |
| Bi 50.0, Pb 28.0, Sn 22.0 | 109 | nu | metalul lui Rose |
| Bi 56.5, Pb 43.5 | 125 | da | |
| Bi 58 , Sn 42 | 139 | da | |
| In 100 | 157 | da | |
| Sn 62.3, Pb 37.7 | 183 | da | |
| Sn 63.0, Pb 37.0 | 183 | nu | Eutectic solder |
| Sn 91.0, Zn 9.0 | 198 | da | |
| Sn 92.0, Zn 8.0 | 199 | nu | staniu folie |
Note
- Oshe, Ed. R.W., "Handbook of Thermodynamic and Transport Properties of Alkali Metals", Oxford. UK, Blackwell Scientific Publications Ltd, 1985, p. 987
Legături externe
This article is issued from Wikipedia. The text is licensed under Creative Commons - Attribution - Sharealike. Additional terms may apply for the media files.